'''Procedure for bringing new user resist bottles into the cleanroom:'''
'''Procedure for bringing new user resist bottles into the cleanroom:'''
#''Outside the cleanroom'': Find a blue-capped glass bottle in the cupboard next to office 055 in 346
#''Outside the cleanroom'': Find a blue-cap glass bottle in the cupboard next to office 055 in building 346
#''Gowning'': Clean the bottle in gowning
#''Gowning'': Clean the bottle in gowning
#*Clean it thoroughly on the outside with water or alcohol