Jump to content

Specific Process Knowledge/Bonding/Eutectic bonding: Difference between revisions

From LabAdviser
Rkch (talk | contribs)
Sifkle (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:photolith@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Bonding/Eutectic_bonding click here]'''
'''Feedback to this page''': '''[mailto:photolith@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Bonding/Eutectic_bonding click here]'''
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''


==Eutectic Bonding==
==Eutectic Bonding==

Revision as of 08:24, 6 February 2023

Feedback to this page: click here Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

Eutectic Bonding

Eutectic bonding depends on a formation of an eutecticum in the bond interphase. This makes bonding of two substates by use of eg. a AuSi eutecticum possible at temperatures much lower than the actual melting points of either of the two (in this case bonding can be done at around 390oC). The bonding strecth is quite good, but far from as good as anodic bonding. Different eutectica have a different eutectic (bonding) temperature


Eutecticum Eutectic temperature Bonding temperature in Wafer Bonder 02
AuSi 365oC 390oC
AuSn <300oC 300oC
AuSnNi . .