Jump to content

Specific Process Knowledge/Bonding/Imprinter 02: Difference between revisions

From LabAdviser
Sifkle (talk | contribs)
No edit summary
Sifkle (talk | contribs)
No edit summary
Line 2: Line 2:


'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
'''All links to Labmanager requires login'''
'''All links to Labmanager requires login'''



Revision as of 08:22, 6 February 2023

Feedback to this page: click here

Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

All links to Labmanager requires login

The Imprinter 02 is a system for bonding. 3 different types of Polymer bonds bonding can be done: PMMA, SU8 and BCB. It not is possible to mechanically align the wafers. It is also possible to process pieces.

The user manual, quality control procedure and results, user APV(s), and contact information can be found in LabManager: Equipment info in LabManager



Overview of the performance of the Imprinter 02 and some process related parameters

Purpose Bonding
  • PMMA bonding
  • SU-8 bonding
  • BCB bonding
Performance Alignment accuracy
  • Flat alingment by eye
Process parameter range Process Temperature
  • Room temperature to 240oC
Process pressure
  • ~1mbar - 1000mbar
Piston Force
  • Atm - 6000 mbar.
Substrates Batch size
  • One wafer per run
  • Pieces
Substrate material allowed
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
  • InP
  • GaAs
Material allowed on the substrate
  • Silicon oxide
  • Silicon (oxy)nitride
  • Poly Silicon
  • PMMA
  • SU-8
  • BCB
  • Metals: Au, Sn, Ag, Al, Ti..