Specific Process Knowledge/Etch/ICP Metal Etcher/silicon: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 4: | Line 4: | ||
== Silicon etching on the ICP Metal Etcher == | == Silicon etching on the ICP Metal Etcher == | ||
<!--Page reviewed by jmli 2/2-2023 --> | |||
{{Template:Author-jmli1}} | |||
In the primary silicon etcher at Nanolab, the [[Specific Process Knowledge/Etch/DRIE-Pegasus|DRIE-Pegasus]], silicon is etched using a fluorine based plasma (with SF<sub>6</sub> as etch gas). Silicon is also etched by chlorine and bromine. | In the primary silicon etcher at Nanolab, the [[Specific Process Knowledge/Etch/DRIE-Pegasus|DRIE-Pegasus]], silicon is etched using a fluorine based plasma (with SF<sub>6</sub> as etch gas). Silicon is also etched by chlorine and bromine. | ||