== Effects on Process A of showerhead change in December 2014 == | == Effects on Process A of showerhead change in December 2014 == | ||
{{Template:Author-jmli1}} | |||
<!--Checked for updates on 2/02-2023 - ok/jmli --> | |||
The effects of [[Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange|changing of the showerhead in December 2014]] was investigated. Patterned wafers were processed before and after and the profile of the etched features were inspected in SEM. Click on the numbers in the 'Runs' column below to see the profiles. | The effects of [[Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange|changing of the showerhead in December 2014]] was investigated. Patterned wafers were processed before and after and the profile of the etched features were inspected in SEM. Click on the numbers in the 'Runs' column below to see the profiles. | ||