Line 165: Line 165:
**Select 'Use e.s.d. for weight factor' (estimated standard deviation).
**Select 'Use e.s.d. for weight factor' (estimated standard deviation).
**Chose if width corrections is to be used.
**Chose if width corrections is to be used.
For more info on these see the manual by clicking ? in the right panel for the plugin (Crystallite Size and Strain, Lattice Parameter Refinement, or %Crystallinity) or in [http://labmanager.dtu.dk/view_binary.php?fileId=4247 LabManager]
For more info on these see the manual by clicking ? in the right panel for the plugin (Crystallite Size and Strain, Lattice Parameter Refinement, or %Crystallinity) or in [http://labmanager.dtu.dk/view_binary.php?fileId=4247 LabManager] - requires login
 
===Comprehensive Analysis/Lattice parameter refinement===
===Comprehensive Analysis/Lattice parameter refinement===
For Lattice parameter refinement, follow the steps for search and match. After phase identification do the following.
For Lattice parameter refinement, follow the steps for search and match. After phase identification do the following.