Specific Process Knowledge/Thin film deposition/Deposition of Tin: Difference between revisions

From LabAdviser
Reet (talk | contribs)
Eves (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:pvd@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Tin&action=edit click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Tin click here]'''
 
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>


== Tin deposition ==
== Tin deposition ==

Revision as of 17:10, 1 February 2023

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal

Tin deposition

Tin can be deposited by e-beam evaporation. It was evaporated in the Alcatel e-beam evaporator, which is decommissioned, but has not yet been evaporated in the Temescal e-beam evaporator which we have now (September 2021). Please contact the Thin Film group if you would like to deposit tin.

E-beam evaporation (Temescal)
General description E-beam deposition of Sn

(line-of-sight deposition)

Pre-clean Ar ion clean
Layer thickness 10Å to 1µm*
Deposition rate 1Å/s to 10Å/s
Pre-clean Ar ion bombardment
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • small pieces
Allowed materials
Comment Tin has not yet been deposited in the Temescal to date (May 2022).

Please contact the Thin Film group if you would like us to develop the process.

* For thicknesses above 600 nm permission is required.