===Definition of <110> alignment structures===
===Definition of <110> alignment structures===


The etch rate dependence on the crystallographic planes can be used to determine the <110> crystal directions with high precision (better than +/- 0.05 <sup>o</sup>). A fast method for doing this, using the symmetric under-cutting behavior around but not at the <110>-directions, was described by https://iopscience.iop.org/article/10.1088/0960-1317/6/2/011/meta. [[https://iopscience.iop.org/article/10.1088/0960-1317/6/2/011/meta|Mattias Vangbo and Ylva Bäcklund 1996 J. Micromech. Microeng. '''6''', 279-284]]  High-precision control of the <110>-direction during alignment can be necessary in order to control the dimensions of KOH-etched structures (e.g. precise control of V-groove dimensions).  
The etch rate dependence on the crystallographic planes can be used to determine the <110> crystal directions with high precision (better than +/- 0.05 <sup>o</sup>). A fast method for doing this, using the symmetric under-cutting behavior around but not at the <110>-directions, was described by [https://iopscience.iop.org/article/10.1088/0960-1317/6/2/011/meta Mattias Vangbo and Ylva Bäcklund 1996 J. Micromech. Microeng. '''6''', 279-284]. High-precision control of the <110>-direction during alignment can be necessary in order to control the dimensions of KOH-etched structures (e.g. precise control of V-groove dimensions).  


<br clear="all" />
<br clear="all" />