Specific Process Knowledge/Lithography/EBeamLithography/JEOLPatternPreparation: Difference between revisions

Thope (talk | contribs)
Thope (talk | contribs)
Line 30: Line 30:
Global alignment '''(SETWFR)''' has a rough scan and a fine scan setting. Initially the mark is found using the rough scan setting, which is set to scan a long distance, typically 500 µm. Once the mark is located the machine will continue with the fine scan setting which will tyipcally scan <10 µm. In order for the machine to see the mark on the rough scan setting the cross must have sufficient width
Global alignment '''(SETWFR)''' has a rough scan and a fine scan setting. Initially the mark is found using the rough scan setting, which is set to scan a long distance, typically 500 µm. Once the mark is located the machine will continue with the fine scan setting which will tyipcally scan <10 µm. In order for the machine to see the mark on the rough scan setting the cross must have sufficient width


[[File:RoughFineScan.png|300px|center|frameless]]
[[File:RoughFineScan.png|250px|center|frameless]]