| Line 36: | Line 36: | ||
The recommended development speed in 2.38% TMAH (AZ 4726 MIF) for AZ 4562 is 2 µm/min. A 6.2µm resist film thus requires ~3 min development, recommended as three separate 60 s puddles. | The recommended development speed in 2.38% TMAH (AZ 4726 MIF) for AZ 4562 is 2 µm/min. A 6.2µm resist film thus requires ~3 min development, recommended as three separate 60 s puddles. 10 µm AZ 4562 has successfully been developed using 4 x 60 s development. | ||