Jump to content

Specific Process Knowledge/Thermal Process/RTP Annealsys: Difference between revisions

Indiogo (talk | contribs)
Tag: Manual revert
Indiogo (talk | contribs)
Line 197: Line 197:
<br clear = "all" />
<br clear = "all" />


'''Up''' = Facing the chamber; '''Up, covered''' = facing the chamber, covered with an identical (in size) Si chip during the process; '''Flipped''' = Facing the carrier wafer; '''HF dip''' = 30s-HF chemical bath, immediately prior to processing.
'''Up''' = Facing the chamber; '''Up, covered''' = facing the chamber, covered with an identical (in size) Si chip during the process;
'''Flipped''' = Facing the carrier wafer; '''HF dip''' = 30s-HF chemical bath, immediately prior to processing.


==== RTH ====
==== RTH ====