Jump to content

Specific Process Knowledge/Lithography/5214E: Difference between revisions

Jehem (talk | contribs)
Jehem (talk | contribs)
Line 6: Line 6:
[[Image:5214Espincurves.JPG|500x500px|thumb|Spin curves for AZ 5214E using a 30s spin-off, and a 60s@90°C softbake]]
[[Image:5214Espincurves.JPG|500x500px|thumb|Spin curves for AZ 5214E using a 30s spin-off, and a 60s@90°C softbake]]


'''Typical spin parameers:'''
'''Typical spin parameters:'''
*Spin off: 30-60 s
*Spin off: 30-60 s
*Soft bake: 60s @ 90°C
*Soft bake: 60s @ 90°C