Specific Process Knowledge/Lithography/Resist/UVresist: Difference between revisions
Appearance
| Line 957: | Line 957: | ||
'''Dehydration reducing measures used for testing AZ MiR 701:'''<br> | '''Dehydration reducing measures used for testing AZ MiR 701:'''<br> | ||
The CDA used for the pneumatic autofocus will dehydrate the resist. To reduce this effect, the writehead is parked far away from the write area while setting up the job for at least a few minutes, before starting the exposure. | The CDA used for the pneumatic autofocus will dehydrate the resist. To reduce this effect, the writehead is parked far away from the write area while setting up the job for at least a few minutes, before starting the exposure. | ||
<br clear="all" /> | |||
==Exposure dose when using AZ 351B developer (NaOH)== | ==Exposure dose when using AZ 351B developer (NaOH)== | ||