==The Set-Up==
==The Set-Up==


[[File:Set up.png|700px|thumb|right|Schematic representation of the rapid thermal processor set-up profile view. The substrate (in green) rests on top of three quartz pins, supported by a quartz holder (in black). The drawing is not to scale.]]
[[File:Set up.png|690px|thumb|right|Schematic representation of the rapid thermal processor set-up profile view. The substrate (in green) rests on top of three quartz pins, supported by a quartz holder (in black). The drawing is not to scale.]]


The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock.
The RTP Annealsys system is divided into two main parts: the process chamber and the loadlock.