Created page with "==Spin Coater: Gamma UV== 400px|right|thumb|Spin Coater: Gamma UV in E-5 '''Feedback to this section''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/Coaters#Spin_Coater:_Gamma_UV click here]''' ''Coater comparison table'' Spin Coater: Gamma UV was insta..." |
|||
| Line 2: | Line 2: | ||
[[image:SpinCoaterGammaUV.jpg|400px|right|thumb|Spin Coater: Gamma UV in E-5]] | [[image:SpinCoaterGammaUV.jpg|400px|right|thumb|Spin Coater: Gamma UV in E-5]] | ||
Spin Coater: Gamma UV was installed at DTU Nanolab in March 2015. It is a Gamma 2M cluster from Süss MicroTec with spin coating, vapour priming, and baking modules. The system handles 4" and 6" wafers without size conversion, and can be set up to handle 2" or 8". | Spin Coater: Gamma UV was installed at DTU Nanolab in March 2015. It is a Gamma 2M cluster from Süss MicroTec with spin coating, vapour priming, and baking modules. The system handles 4" and 6" wafers without size conversion, and can be set up to handle 2" or 8". | ||
Revision as of 14:32, 27 January 2023
Spin Coater: Gamma UV

Spin Coater: Gamma UV was installed at DTU Nanolab in March 2015. It is a Gamma 2M cluster from Süss MicroTec with spin coating, vapour priming, and baking modules. The system handles 4" and 6" wafers without size conversion, and can be set up to handle 2" or 8".
The coater is equipped with 3 different resists lines:
- AZ MiR 701
- AZ nLOF 2020
- AZ 5214E
and
- 1 syringe, which can be used for various resists.
The processes that are available on the system are developed by Nanolab. Upon request, it is possible to establish new processes. Use of the syringe requires special training, and would as a starting point require batches in excess of 20 wafers.
The user manual, quality control procedures and results, user APVs, and contact information can be found in LabManager
Process information
| Purpose |
| |
|---|---|---|
| Resist |
| |
| Performance | HMDS contact angle |
60 - 80° |
| Coating thickness |
| |
| Process parameters | Priming temperature |
120 °C |
| Spin speed |
10 - 6000 rpm | |
| Spin acceleration |
10 - 10000 rpm/s | |
| Hotplate temperature |
25 - 200 °C | |
| Cool plate temperature |
21 °C | |
| Substrates | Substrate size |
|
| Allowed materials |
Silicon and glass No resist or crystalbond allowed in the HMDS module | |
| Batch |
1 - 25 |
1) Requires tool change.