=== Pillars ===
=== Pillars ===


Using patterned samples of 1 μm pillars with 50 nm of Al<sub>2</sub>O<sub>3</sub>. After the tests, approximately 20nm of Al<sub>2</sub>O<sub>3</sub> were still intact.
Using patterned samples of 1 μm pillars with 50 nm of Al<sub>2</sub>O<sub>3</sub>. After the tests, approximately 32nm of Al<sub>2</sub>O<sub>3</sub> were still intact.
<br clear="all" />
<br clear="all" />
{| border="1" style="text-align: center; width: 650px; height: 200px"
{| border="1" style="text-align: center; width: 650px; height: 200px"