Specific Process Knowledge/Thin film deposition/Deposition of Silicon Carbide: Difference between revisions
Appearance
No edit summary |
|||
| Line 5: | Line 5: | ||
== Deposition of Silicon Carbide == | == Deposition of Silicon Carbide == | ||
Sicicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using Sputter-System (Lesker): | Sicicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using [[Specific Process Knowledge/Thin film deposition/Lesker|Sputter-System (Lesker)]]: | ||
*[[/Deposition of SiC in Sputter-System Lesker|Deposition of SiC in Sputter-System (Lesker)]] | *[[/Deposition of SiC in Sputter-System Lesker|Deposition of SiC in Sputter-System (Lesker)]] | ||
Revision as of 20:46, 20 December 2022
Feedback to this page: film deposition/Deposition of Silicon Carbide click here
Deposition of Silicon Carbide
Sicicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using Sputter-System (Lesker):