Line 278: Line 278:
|-  
|-  
|Deposition rate
|Deposition rate
|10 Å/s (change to 2 Å/s from October 2022 as it gives less particles)
|was at 10 Å/s (change to 2 Å/s from October 2022 as it gives less particles)
|-
|-
|Thickness