Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Molybdenum: Difference between revisions

From LabAdviser
Paphol (talk | contribs)
No edit summary
Reet (talk | contribs)
Line 70: Line 70:
|-style="background:WhiteSmoke; color:black"
|-style="background:WhiteSmoke; color:black"
! Comment
! Comment
| As of August 2018, Mo has not yet been deposited in the Temescal.  
| As of August 2022, Mo has not yet been deposited in the Temescal.  
Please contact the Thin Film group to develop a process.
Please contact the Thin Film group to develop a process.
|
|

Revision as of 17:21, 9 September 2022

Feedback to this page: click here


Molybdenum deposition

Molybdenum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.

E-beam evaporation (Temescal) Sputter deposition (Lesker)
General description E-beam deposition of Mo

(line-of-sight deposition)

Sputter deposition of Mo

(not line-of-sight)

Pre-clean Ar ion source RF Ar clean
Layer thickness 10Å to 0.2 µm* 10Å to 500 Å
Deposition rate 1Å/s to 10Å/s Depends on process parameters, roughly about 1 Å/s
Batch size
  • Up to 4x6" wafers
  • Up to 3x8" wafers (ask for holder)
  • Many smaller pieces
  • Pieces or
  • 1x4" wafer or
  • 1x6" wafer
Allowed materials
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
Comment As of August 2022, Mo has not yet been deposited in the Temescal.

Please contact the Thin Film group to develop a process.


* Depending on the amount of heating during Mo deposition, which we will discover during process development.