Tantalum can be deposited by e-beam evaporation and sputter deposition. In the chart below you can compare the different deposition equipment. | Tantalum can be deposited by e-beam evaporation and sputter deposition. In the chart below you can compare the different deposition equipment. | ||
You can read more about Ta sputter deposition [[Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Tantalum/Sputtering of Ta|here]]. | You can read more about Ta sputter deposition using Sputter-System(Lesker) [[Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Tantalum/Sputtering of Ta|here]]. | ||
Revision as of 14:03, 31 August 2022
Feedback to this page: click here
Tantalum deposition
Tantalum can be deposited by e-beam evaporation and sputter deposition. In the chart below you can compare the different deposition equipment.
You can read more about Ta sputter deposition using Sputter-System(Lesker) here.
| E-beam evaporation (Temescal) | Sputter (Lesker) | Sputter deposition (Sputter-system Metal-Oxide (PC1) and Sputter-system Metal-Nitride (PC3)) | |
|---|---|---|---|
| General description | E-beam deposition of Ta
(line-of-sight deposition) |
Sputter deposition of Ta
(not line-of-sight) |
Sputter deposition of Ta
(not line-of-sight) |
| Pre-clean | Ar ion source | RF Ar clean | RF Ar clean |
| Layer thickness | 10Å to 0.2 µm* | 10Å to ? | 10Å to ? |
| Deposition rate | 0.5Å/s to 10Å/s | ~0.3Å/s | Not been tested |
| Batch size |
|
|
|
| Allowed materials |
|
|
|
| Comment | Tantalum deposition heats the chamber* | 3-inch Ta target |
* The max thickness is limited to 200 nm as Ta deposition heats the chamber. If you wish to deposit more than that, it has to be done in several steps. The temperature on the back of a Si wafer rose to above 160 °C during deposition of 40 nm Ta even when using a cooling plate. If you wish to e-beam deposit Ta, please contact the Thin film group.