* 0.0232 nm/cycle on a high aspect ratio structures | * 0.0232 nm/cycle on a high aspect ratio structures | ||
| | | | ||
* about | * about 0.12 nm/s, depends on sputtering parameters, check processlog in LabManager | ||
| | | | ||
* up to 0.0625 nm/s on a flat sample | * up to 0.0625 nm/s on a flat sample | ||