Specific Process Knowledge/Thin film deposition/Deposition of AZO: Difference between revisions
Appearance
added new sputter equipment |
No edit summary |
||
| Line 50: | Line 50: | ||
| | | | ||
*Many smaller samples | *Many smaller samples | ||
*Up to 10x4" or 6" wafers | *Up to 10x4" or 6" wafers (Cassette load in the LL) | ||
| | | | ||
*Pieces or | *Pieces or | ||
Revision as of 09:07, 30 August 2022
Feedback to this page: click here
AZO can be deposited by sputtering or atomic layer deposition (ALD). In sputter-deposition of AZO, we use an AZO target that may be RF-sputtered or reactively DC-sputtered. You can also co-deposit Al and ZnO. Note that in multipurpose sputter systems such as ours it may be difficult to obtain low enough contamination for high-quality AZO. Talk to Nanolab staff or your colleagues if you would like to locate a sputter system that can be dedicated to AZO-deposition.
In the chart below you can compare the different deposition equipment available here at Nanolab:
| Sputter deposition Sputter-system Metal-Oxide(PC1) | Sputter deposition (Sputter-System(Lesker)) | Atomic layer deposition (ALD Picosun R200) | |
|---|---|---|---|
| General description |
|
|
|
| Pre-clean | RF Ar clean | RF Ar clean | |
| Layer thickness | few nm to ? hundreds of nm* | 10Å to 5000Å* | 0 to 1000 Å |
| Deposition rate | Depending on process parameters. | Depending on process parameters, e.g., 0.3 Å/s reactive DC-sputtering (see process log for details) | Depending on temperature |
| Batch size |
|
|
|
| Allowed materials |
|
|
|
| Comment |
|
|
* For thicknesses above 200 nm permission is required. Write to thinfilm@nanolab.dtu.dk.