Specific Process Knowledge/Lithography/EBeamLithography/eLINE: Difference between revisions
Appearance
| Line 21: | Line 21: | ||
We recommend all EBL users to do a dose test prior to exposing samples of significant value. As a starting point you can consider to use the Demo.csf provided on the tool. This pattern is available in the auto generated user folder. The pattern consist of areas, curved elements, lines and dots as shown below. LINK TO PAGE WITH MORE INFO. | We recommend all EBL users to do a dose test prior to exposing samples of significant value. As a starting point you can consider to use the Demo.csf provided on the tool. This pattern is available in the auto generated user folder. The pattern consist of areas, curved elements, lines and dots as shown below. LINK TO PAGE WITH MORE INFO. | ||
[[Image:DoseChip6.png| | [[Image:DoseChip6.png|500x500px|right|thumb|Overview image of the dose test design provided on the tool. Coloring indicates dose modulation.]] | ||
Table of dose to clear on Si substrate: | Table of dose to clear on Si substrate: | ||