Specific Process Knowledge/Etch/ICP Metal Etcher/Chromium: Difference between revisions
Appearance
| Line 43: | Line 43: | ||
|} | |} | ||
<gallery caption="Etching lines in Cr with the Cr etch for 3 min with 300 nm DUV resist ''BGHE@Nanolab Feb 2022''" perrow="5" widths="400px" heights="300px"> | <gallery caption="Etching lines in 100nm Cr with the Cr etch for 3 min with 300 nm DUV resist ''BGHE@Nanolab Feb 2022''" perrow="5" widths="400px" heights="300px"> | ||
Image:S036039pro_34.jpg | Image:S036039pro_34.jpg | ||