Specific Process Knowledge/Thin film deposition: Difference between revisions
m added diamond as a material you can make under semiconductors |
|||
| Line 13: | Line 13: | ||
| align="left" valign="top" style="background:#DCDCDC;"|''' Transparent conductive oxides''' | | align="left" valign="top" style="background:#DCDCDC;"|''' Transparent conductive oxides''' | ||
| align="left" valign="top" style="background:LightGray"|''' Polymers''' | | align="left" valign="top" style="background:LightGray"|''' Polymers''' | ||
| align="left" valign="top" style="background:#DCDCDC;"|''' Multilayers''' | |||
|-valign="top" | |-valign="top" | ||
Revision as of 17:16, 11 January 2022
Feedback to this page: click here
Choose material to deposit
| Semiconductors | Oxides | Nitrides | Metals | Alloys | Transparent conductive oxides | Polymers | Multilayers |
|
Aluminium Oxide (Al2O3)
|
Silicon Nitride - and oxynitride
|
Aluminium
|
AlCu And an electroceramic: YSZ (Yttrium stabilized zirconia) |
ITO (Tin doped Indium Oxide) |
SU-8 |
Oh no! My material is not on the list! Please contact the Thin Film group if you would like to inquire about a material that is not mentioned here.
Choose deposition equipment
| PVD | LPCVD | PECVD | ALD | Coaters | Others
|
|
|
|
|
See the Lithography/Coaters page for coating polymers |
|