CasaXPS cannot read the *.vgd files that are generated by Avantage when a spectrum is recorded. All data from Avantage that you wish to analyze using CasaXPS must therefore be manually exported from Avantage. Below is a procedure on how to do this.
CasaXPS cannot read the *.vgd files that are generated by Avantage when a spectrum is recorded. All data from Avantage that you wish to analyze using CasaXPS must therefore be manually exported from Avantage. Below is a procedure on how to do this.


# You have to run the file called ''DataSpace_BAtchDump.exe'' that is a part of the Avantage installation. This means that you can run it on the K-Alpha, the Nexsa or your own computer (provided that Avantage is installed on your own PC). On the K-Alpha and Nexsa computers a shortcut labelled 'Export data to CasaXPS' has been put on the deskto[[Image:Xport2casa-a.jpg |right|x300px]].  
# You have to run the file called ''DataSpace_BAtchDump.exe'' that is a part of the Avantage installation. This means that you can run it on the K-Alpha, the Nexsa or your own computer (provided that Avantage is installed on your own PC). On the K-Alpha and Nexsa computers a shortcut labelled 'Export data to CasaXPS' has been put on the desktop [[Image:Xport2casa-a.jpg |right|x300px]]. Depending on the Windows installation the file should be in the folder  
Depending on the Windows installation the file should be in the folder  
## C:\Program Files\Thermo\Avantage\Bin\ or
## C:\Program Files\Thermo\Avantage\Bin\ or
## C:\Program Files (86)\Thermo\Avantage\Bin\
## C:\Program Files (86)\Thermo\Avantage\Bin\
# Running ''DataSpace_BAtchDump.exe'' will open the window
# Running ''DataSpace_BAtchDump.exe'' will open the window

Revision as of 15:25, 18 November 2021

How to export data generated by Avantage to CasaXPS

CasaXPS cannot read the *.vgd files that are generated by Avantage when a spectrum is recorded. All data from Avantage that you wish to analyze using CasaXPS must therefore be manually exported from Avantage. Below is a procedure on how to do this.

  1. You have to run the file called DataSpace_BAtchDump.exe that is a part of the Avantage installation. This means that you can run it on the K-Alpha, the Nexsa or your own computer (provided that Avantage is installed on your own PC). On the K-Alpha and Nexsa computers a shortcut labelled 'Export data to CasaXPS' has been put on the desktop
    . Depending on the Windows installation the file should be in the folder
    1. C:\Program Files\Thermo\Avantage\Bin\ or
    2. C:\Program Files (86)\Thermo\Avantage\Bin\
  2. Running DataSpace_BAtchDump.exe will open the window