== Deposition of Nb == | == Deposition of Nb == | ||
Niobium can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the deposition equipment | Niobium can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the deposition equipment. | ||
{| border="1" cellspacing="0" cellpadding="3" | {| border="1" cellspacing="0" cellpadding="3" | ||
Revision as of 14:46, 3 October 2021
Feedback to this page: click here
Deposition of Nb
Niobium can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the deposition equipment.
| E-beam evaporation (Temescal) | Sputter deposition (Lesker) | |
|---|---|---|
| General description | E-beam deposition of Nb
(line-of-sight deposition) |
Sputter deposition of Nb
(not line-of-sight deposition) |
| Pre-clean | Ar ion bombardment | RF Ar clean |
| Layer thickness | 10Å to 1µm* | 10Å to 1µm** |
| Deposition rate | 0.5Å/s to 3Å/s | ~1Å/s |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment | Substrates get heated during the deposition.
For 100 nm Nb at 2 Å/s, the substrate reached about 105 °C. |
* To deposit layers thicker than 600 nm permission is required to ensure that there is enough metal (contact metal@danchip.dtu.dk)
** To deposit layers thicker than 200 nm permission is required to ensure that there is enough metal (contact metal@danchip.dtu.dk)