Removal of native oxide is a part of the RCA cleaning procedure. See the [[Specific Process Knowledge/Wafer cleaning/RCA|RCA]] page for further details. The HF/BHF baths in the RCA bench bath must only be used during the RCA cleaning procedure. For removal of oxide of processed wafers that is not getting a full RCA clean the other HF/BHF baths can be used. Please | Removal of native oxide is a part of the RCA cleaning procedure. See the [[Specific Process Knowledge/Wafer cleaning/RCA|RCA]] page for further details. The HF/BHF baths in the RCA bench bath must only be used during the RCA cleaning procedure. For removal of oxide of processed wafers that is not getting a full RCA clean the other HF/BHF baths can be used. Please see the [[Specific Process Knowledge/Etch/Wet Silicon Oxide Etch (BHF)|oxide etch]] page for more details. | ||
Revision as of 14:49, 19 August 2021
Feedback to this page: click here
Removal of native oxide is a part of the RCA cleaning procedure. See the RCA page for further details. The HF/BHF baths in the RCA bench bath must only be used during the RCA cleaning procedure. For removal of oxide of processed wafers that is not getting a full RCA clean the other HF/BHF baths can be used. Please see the oxide etch page for more details.