Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/SIMS settings: Difference between revisions
No edit summary |
No edit summary |
||
Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/IBE⁄IBSD_Ionfab_300/SIMS_settings click here]''' | ||
''Made by bghe@nanolab in 2015'' | ''Made by bghe@nanolab in 2015'' |
Revision as of 15:46, 18 August 2021
Feedback to this page: click here
Made by bghe@nanolab in 2015
SIMS setting for different materials | ||
Lower plate | Upper plate | |
---|---|---|
Ti | -1 | |
Si | -1 | (2) |
Al | -1 | 1 |
Cr | -1 | |
Ni | -6 |