PECVD nitride can be deposited in one of the [[Specific Process Knowledge/Thin film deposition/PECVD|PECVD]] systems. You can run 1-3 wafers at a time depending on which one of the PECVD's you use. The deposition takes place at 300 degrees Celcius. This can be  off importance for some applications but it gives a less dense film and the stoichiometry is on the following form: Si<sub>x</sub>N<sub>y</sub>H<sub>z</sub>. The step coverage and thickness uniformity of the film is not as good as for the LPCVD nitride. In one of our PECVD systems (PECVD3) we allow small amounts of metal on the wafers entering the system, this is not allowed in the LPCVD and in the other PECVD (PECVD1).
PECVD nitride can be deposited in one of the [[Specific Process Knowledge/Thin film deposition/PECVD|PECVD]] systems. You can run 1-3 wafers at a time depending on which one of the PECVD's you use. The deposition takes place at 300 degrees Celcius. This can be  off importance for some applications but it gives a less dense film and the stoichiometry is on the following form: Si<sub>x</sub>N<sub>y</sub>H<sub>z</sub>. The step coverage and thickness uniformity of the film is not as good as for the LPCVD nitride. In one of our PECVD systems (PECVD3) we allow small amounts of metal on the wafers entering the system, this is not allowed in the LPCVD and in the other PECVD (PECVD1).


==comparison of LPCVD and PECVD for silicon nitride deposition==
{| border="1" cellspacing="0" cellpadding="3" align="center"
!
! LPCVD
! PECVD
|-
| Stoichiometry
|
*Si<sub>3</sub>N<sub>4</sub>
*SRN
SRN: Silicon rich nitride
|
*Si<sub>x</sub>N<sub>y</sub>H<sub>z</sub>
*Si<sub>x</sub>O<sub>y</sub>N<sub>z</sub>H<sub>v</sub>
Can be doped with boron, phosphorus or germanium
|-
|Film thickness
|
*Si<sub>3</sub>N<sub>4</sub>:~50Å - ~3000Å
*SRN: ~50Å - ~10000Å
|
*~40nm - 10µm
|-
|}


==Choose deposition technique==
==Choose deposition technique==
*[[/Deposition of Silicon Nitride using LPCVD|Deposition of Silicon Nitride using LPCVD]]
*[[/Deposition of Silicon Nitride using LPCVD|Deposition of Silicon Nitride using LPCVD]]
*[[/Deposition of Silicon Nitride using PECVD|Deposition of Silicon Nitride using PECVD]]
*[[/Deposition of Silicon Nitride using PECVD|Deposition of Silicon Nitride using PECVD]]