Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/Isotropic/Isoslow7: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''':
'''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/Isotropic/Isolslow7 click here]'''
<!--Checked for updates on 30/7-2018 - ok/jmli -->
<!--Checked for updates on 30/7-2018 - ok/jmli -->
<!--Checked for updates on 5/10-2020 - ok/jmli -->


{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"
{| border="2" cellpadding="0" cellspacing="0" style="text-align:center;"

Revision as of 08:45, 5 October 2020

Feedback to this page: click here


Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
28/2-2014 4" travka50 wafer 1.5 µm AZ Si / 50 % Pegasus/jmli 1 minute TDESC clean + MU runs jml/isotropic/isoslow7 1:00 minutes S003900 Bottom fine!!