Line 149: Line 149:


It is possible to make perfect capacitors with oxide thicknesses down to and including 5 nm and possibly even thinner, although the failure rate increases. Bear in mind, though that each structure measured here has an area of 8 mm<sup>2</sup> - for a 1 mm<sup>2</sup> structure the failure rate would be much lower, assuming the short circuits are not located on the sides of the structures.
It is possible to make perfect capacitors with oxide thicknesses down to and including 5 nm and possibly even thinner, although the failure rate increases. Bear in mind, though that each structure measured here has an area of 8 mm<sup>2</sup> - for a 1 mm<sup>2</sup> structure the failure rate would be much lower, assuming the short circuits are not located on the sides of the structures.
[[Image:Lesker_Impedance_Bjarke.png|600px|alt text]]