LabAdviser/314/Preparation 314-307/Coating: Difference between revisions
Appearance
No edit summary |
|||
| Line 19: | Line 19: | ||
[http://labmanager.dtu.dk/view_binary.php?fileId=3020 Manual] | [http://labmanager.dtu.dk/view_binary.php?fileId=3020 Manual] | ||
[[File: | [[File:Quorum coater.jpg|400px|left|thumb|Location Building 314, Prep Room 03]]<br /> | ||
<br clear="all" /> | <br clear="all" /> | ||
| Line 27: | Line 27: | ||
[http://cressington.com/spec_208hr.html Brochure] | [http://cressington.com/spec_208hr.html Brochure] | ||
[[File:IMG_3685.JPG|250px|left|thumb|Location Building 314, Prep Room 01]]<br /> | [[File:IMG_3685.JPG|250px|left|thumb|Quorum Q150T Sputter Coater Location Building 314, Prep Room 01]]<br /> | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 15:20, 30 September 2020
Feedback to this page: click here
Coaters & Accessories
Cressington 208 Carbon Coater
Quorum Q150T Sputter Coater and Glow discharge