Silicon wafers are prepared with 1.5 μm thick resist patterns (AZ MIR 701 DUV resist from MicroChemicals) and exposed using a maskless aligner (MLA150, Heidelberg) to create patterns above 400 nm. Below are some SEM images of BSi nanostructures achieved by the modified CORE process:
Silicon wafers are prepared with 1.5 μm thick resist patterns (AZ MIR 701 DUV resist from MicroChemicals) and exposed using a maskless aligner (MLA150, Heidelberg) to create patterns above 400 nm. Below are some SEM images of BSi nanostructures achieved by the modified CORE process:


[[File:Figure_8.png|800px|left|thumb|'''''Submicron silicon trenches and lines derived from the fine-tuned CORE sequence.''''']]
[[File:BSi free.png|800px|left|thumb|''''' 1 µm silicon pillars etched with a BSi-free recipe''''']]