Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-2/Si Nano etching: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 25: | Line 25: | ||
[[File:Fig 13c.png|800px|left|thumb|'''''Submicron silicon pillars derived from the fine-tuned CORE sequence.''''' ] | [[File:Fig 13c.png|800px|left|thumb|'''''Submicron silicon pillars derived from the fine-tuned CORE sequence.''''' ]] | ||
[[File:Fig 13d - 1.png|800px|left|thumb|'''''Notch-free nanostructures in SOI material derived from the fine-tuned CORE sequence.(Left) Grating with 80 nm periodicity. (Right) RIE lag test structure between 30 and 100 nm.''''']] | [[File:Fig 13d - 1.png|800px|left|thumb|'''''Notch-free nanostructures in SOI material derived from the fine-tuned CORE sequence.(Left) Grating with 80 nm periodicity. (Right) RIE lag test structure between 30 and 100 nm.''''']] | ||