Specific Process Knowledge/Lithography/Aligners/Aligner: Maskless 02 processing: Difference between revisions
Appearance
| Line 297: | Line 297: | ||
At the end of substrate detection, the sample is scanned twice along the bottom edge (flat), in order to determine the substrate rotation. This angle will be presented in the exposure panel along with the option to expose the design rotated in order to compensate for this angle, i.e. aligned to the flat/edge of the substrate. | At the end of substrate detection, the sample is scanned twice along the bottom edge (flat), in order to determine the substrate rotation. This angle will be presented in the exposure panel along with the option to expose the design rotated in order to compensate for this angle, i.e. aligned to the flat/edge of the substrate. | ||
'''Result of using "Expose with substrate angle" | '''Result of using "Expose with substrate angle":''' | ||
*Rotation: 0.5±0.2° | *Rotation: 0.5±0.2° | ||
*Centring: | *Centring: | ||
** '''X''' 100±250µm | ** '''X''' 100±250µm | ||
** '''Y''' 200±250µm | ** '''Y''' 200±250µm | ||
Taran Mar 2019, average of 3 4" wafers.<\br> | |||
The error on the flat alignment is surprising when compared to the 0±0.1° measured on Aligner: Maskless 01. The centring, on the other hand, is seen to be within a few hundred µm, without correcting for the flats. | The error on the flat alignment is surprising when compared to the 0±0.1° measured on Aligner: Maskless 01. The centring, on the other hand, is seen to be within a few hundred µm, without correcting for the flats. | ||