'''AZ nLOF 2020''' has also been tested. It seems to work even at 405nm, but the dose is so hign (>10000) that exposure would be slower than Aligner: Maskless 02.
'''AZ nLOF 2020''' has also been tested. It seems to work even at 405nm, but the dose is so high (>10000) that exposure would be slower than Aligner: Maskless 02.