== Overview of the processing options on the XPS Nexsa==
The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze <span title="The only analytical option (that means excluded chillers, factory training courses, UPS etc) not chosen is a vacuum transfer module " >''' ''all'' '''</span>''' but one of the available options into the budget.


{| border="2" cellspacing="0" cellpadding="1" {{table}}
{| border="2" cellspacing="0" cellpadding="1" {{table}}

Revision as of 10:34, 14 April 2020

Overview of the processing options on the XPS Nexsa

The acquisition of an instrument like the Nexsa has to be done through a EU tender process. As a somewhat unexpected result of this process, we were offered the Nexsa at a very favorable price. We were therefore able to squeeze all but one of the available options into the budget.

Publication Techniques and hardware applied Sample types/Materials Abstract: Hover cursor to show
Title Type Author Web of Science XPS UPS ISS REELS Raman Additional options/hardware
Multitechnique Surface Characterization of Organic LED Material Application note P Mack X X X Organic LED's Abstract
Advantages of coincident XPS-Raman in the analysis of mineral oxides species Application note X X TiO2, CaCO3
Spectroscopic analysis of solid oxide fuel cell material with XPS Application note P Mack X
Rapid XPS image acquisition using SnapMap Application note R Simpson X SnapMap
Composition, coverage and band gap analysis of ALD-grown ultra thin films Application note P Mack X X X Band gap Gate dielectrics, HfO2, SiO2
Confirming the layer structure of an organic FET device Application note P Mack X MAGCIS Organic FET's,
Surface analysis of zeolites: An XPS, variable kinetic energy XPS, and low energy ion scattering study Publication SR Bare link X X Zeolites, Metal oxides Abstract
Surface composition analysis by low-energy ion scattering Publication, background H H Brongersma link X Abstract
Monitoring surface metal oxide catalytic active sites with Raman spectroscopy Publication, review I E Wachs link X Metal oxides Abstract
Diffusion of In0.53Ga0.47As elements through hafnium oxide during post deposition annealing Publication W Cabrera link X X TEM HfO2, InGaAs, ALD Abstract
Low energy ion scattering (LEIS). A practical introduction to its theory, instrumentation, and applications Publication, review C V Cushman link X Abstract
HfO2 on MoS2 by Atomic Layer Deposition: Adsorption Mechanisms and Thickness Scalability Publication S McDonnell link X X AFM, ALD HfO2, MoS2 Abstract
Highly Sensitive Detection of Surface and Intercalated Impurities in Graphene by LEIS Publication S Prusa link X graphene Abstract
Reflection electron energy loss spectroscopy for ultrathin gate oxide materials Publication H C Shin link X X Valence band HfZrO4, Abstract
Oxygen accumulation on metal surfaces investigated by XPS, AES and LEIS, an issue for sputter depth profiling under UHV conditions Publication R Steinberger link X X AES, ARXPS, sputter profiles Oxygen on metal surfaces Abstract
Electrochemical Characterization and Quantified Surface Termination Obtained by Low Energy Ion Scattering and X-ray Photoelectron Spectroscopy of Orthorhombic and Rhombohedral LaMnO3 Powders Publication E Symianakis link X X XRD Catalysts, LaMnO3 Abstract
The Thermal Oxidation of TiAlN High Power Pulsed Magnetron Sputtering Hard Coatings as Revealed by Combined Ion and Electron Spectroscopy Publication M Wiesing link X X X Ar sputtering TiAlN Abstract
Electronic structure and energy band gap of poly(9,9-dioctylfluorene) investigated by photoelectron spectroscopy Publication L S Liao link X X Polymer Abstract
Electronic and optical properties of hafnium indium zinc oxide thin film by XPS and REELS Publication Y R Denny link X X Abstract