The table below has been adapted from [http://xdb.lbl.gov/Section1/Sec_1-1.html]. | The table below has been adapted from [http://xdb.lbl.gov/Section1/Sec_1-1.html]. | ||
=Hydrogen (1) to copper (29)= | |||
{| border="2" cellspacing="0" cellpadding="1" {{table}} | {| border="2" cellspacing="0" cellpadding="1" {{table}} | ||
| | | align="center" style="background:#f0f0f0;"|'''Orbital''' | ||
| align="center" style="background:#f0f0f0;"|'''1s''' | |||
| align="center" style="background:#f0f0f0;"|'''2s''' | |||
| align="center" style="background:#f0f0f0;"|'''2p<sub>1/2</sub>''' | |||
| align="center" style="background:#f0f0f0;"|'''2p<sub>3/2</sub>''' | |||
| align="center" style="background:#f0f0f0;"|'''3s''' | |||
| align="center" style="background:#f0f0f0;"|'''3p<sub>1/2</sub>''' | |||
| align="center" style="background:#f0f0f0;"|'''3p<sub>3/2</sub>''' | |||
|- | |- | ||
| ''' 1 H'''||13,6|||||||||||| | | ''' 1 H'''||13,6|||||||||||| | ||
|- | |- | ||
! '''2 He'''||24,6|||||||||||| | |||
|- | |- | ||
| '''3 Li'''||54,7|||||||||||| | | '''3 Li'''||54,7|||||||||||| | ||
|- | |- | ||
! '''4 Be'''||111,5|||||||||||| | |||
|- | |- | ||
| ''' 5 B'''||188|||||||||||| | | ''' 5 B'''||188|||||||||||| | ||
|- | |- | ||
! '''6 C'''||284,2|||||||||||| | |||
|- | |- | ||
| '''7 N'''||409,9||37,3|||||||||| | | '''7 N'''||409,9||37,3|||||||||| | ||
|- | |- | ||
! '''8 O'''||543,1||41,6|||||||||| | |||
|- | |- | ||
| '''9 F'''||696,7|||||||||||| | | '''9 F'''||696,7|||||||||||| | ||
|- | |- | ||
! '''10 Ne'''||870,2||48,5||21,7||21,6|||||| | |||
|- | |- | ||
| '''11 Na'''||1070,8||63,5||30,65||30,81|||||| | | '''11 Na'''||1070,8||63,5||30,65||30,81|||||| | ||
|- | |- | ||
! '''12 Mg'''||1303||88,7||49,78||49,5|||||| | |||
|- | |- | ||
| '''13 Al'''||1559,6||117,8||72,95||72,55|||||| | | '''13 Al'''||1559,6||117,8||72,95||72,55|||||| | ||
|- | |- | ||
! '''14 Si'''||1839||149,7||99,82||99,42|||||| | |||
|- | |- | ||
| '''15 P'''||2145,5||189||136||135|||||| | | '''15 P'''||2145,5||189||136||135|||||| | ||
|- | |- | ||
! '''16 S'''||2472||230,9||163,6||162,5|||||| | |||
|- | |- | ||
| '''17 Cl'''||2822,4||270||202||200|||||| | | '''17 Cl'''||2822,4||270||202||200|||||| | ||
|- | |- | ||
! '''18 Ar'''||3205,9||326,3||250,6||248,4||29,3||15,9||15,7 | |||
|- | |- | ||
|''' 19 K'''||3608,4||378,6||297,3||294,6||34,8||18,3||18,3 | |''' 19 K'''||3608,4||378,6||297,3||294,6||34,8||18,3||18,3 | ||
|- | |- | ||
! '''20 Ca'''||4038,5||438,4||349,7||346,2||44,3||25,4||25,4 | |||
|- | |- | ||
|''' 21 Sc'''||4492||498||403,6||398,7||51,1||28,3||28,3 | |''' 21 Sc'''||4492||498||403,6||398,7||51,1||28,3||28,3 | ||
|- | |- | ||
! '''22 Ti'''||4966||560,9||460,2||453,8||58,7||32,6||32,6 | |||
|- | |- | ||
| '''23 V'''||5465||626,7||519,8||512,1||66,3||37,2||37,2 | | '''23 V'''||5465||626,7||519,8||512,1||66,3||37,2||37,2 | ||
|- | |- | ||
! '''24 Cr'''||5989||696||583,8||574,1||74,1||42,2||42,2 | |||
|- | |- | ||
| '''25 Mn'''||6539||769,1||649,9||638,7||82,3||47,2||47,2 | | '''25 Mn'''||6539||769,1||649,9||638,7||82,3||47,2||47,2 | ||
|- | |- | ||
! '''26 Fe'''||7112||844,6||719,9||706,8||91,3||52,7||52,7 | |||
|- | |- | ||
| '''27 Co'''||7709||925,1||793,2||778,1||101||58,9||59,9 | | '''27 Co'''||7709||925,1||793,2||778,1||101||58,9||59,9 | ||
|- | |- | ||
! '''28 Ni'''||8333||1008,6||870||852,7||110,8||68||66,2 | |||
|- | |- | ||
| '''29 Cu'''||8979||1096,7||952,3||932,7||122,5||77,3||75,1 | | '''29 Cu'''||8979||1096,7||952,3||932,7||122,5||77,3||75,1 | ||
| Line 82: | Line 88: | ||
|} | |} | ||
= Zink (30) to iodine (53) = | |||
{| border="2" cellspacing="0" cellpadding="1" {{table}} | {| border="2" cellspacing="0" cellpadding="1" {{table}} | ||
| Line 153: | Line 159: | ||
|} | |} | ||
=Xenon (54) to gold (79) = | |||
{| border="2" cellspacing="0" cellpadding="1" {{table}} | {| border="2" cellspacing="0" cellpadding="1" {{table}} | ||
| Line 233: | Line 239: | ||
|} | |} | ||
= Mercury (80) to uranium (92)= | |||
{| border="2" cellspacing="0" cellpadding="1" {{table}} | {| border="2" cellspacing="0" cellpadding="1" {{table}} | ||