[[Image:XPS K-Alpha.jpg |frame|left|x300px|The K-Alpha from 2007 is one of the first instruments of this type that was produced.]] | |||
[[Image:XPS Nexsa.png |frame|left|x300px|The Nexsa from 2019 is on the surface very similar to the K-Alpha. It's panels, however, hide a whole range of supplementary techniques.]] | |||
In the basement under the cleanroom two X-ray Photoelectron Spectroscopy (XPS) systems are installed back-to-back in the center of room 904. They are both manufactured by Thermofisher and they enable the users to perform elemental and chemical analysis of samples. The [[Specific Process Knowledge/Characterization/XPS/K-Alpha |XPS K-Alpha]] is a base technique instrument providing XPS analysis. The [[Specific Process Knowledge/Characterization/XPS/Nexsa |XPS Nexsa]] is an upgraded version with all options. | In the basement under the cleanroom two X-ray Photoelectron Spectroscopy (XPS) systems are installed back-to-back in the center of room 904. They are both manufactured by Thermofisher and they enable the users to perform elemental and chemical analysis of samples. The [[Specific Process Knowledge/Characterization/XPS/K-Alpha |XPS K-Alpha]] is a base technique instrument providing XPS analysis. The [[Specific Process Knowledge/Characterization/XPS/Nexsa |XPS Nexsa]] is an upgraded version with all options. | ||