The Cleaver: Lattice Axe is designed for cleaving wafers into smaller pieces. The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5.
The Cleaver: Lattice Axe is designed for cleaving wafers into smaller pieces without leaving any particles on the sample. The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5.


[[File:LatticeAxe placer prøve.JPG|400px]]
[[File:LatticeAxe placer prøve.JPG|400px]]

Revision as of 15:29, 31 March 2020

The Cleaver: Lattice Axe is designed for cleaving wafers into smaller pieces without leaving any particles on the sample. The equipment is placed in the left drawer underneath fumehood 5: Special purposes. When operated the the Cleaver: lattice axe should always be placed inside Fume hood 5.

Approved Materials:

  • Si
  • Quartz
  • Pyrex (Borofloat 33)
  • GaAs
  • InP
  • Sapphire

The LatticeAxe can cleave samples from 100mm down to 10mm. In some cases it can even be used on 150mm samples please contact wetchemistry group for more information