Created page with "'''Procedure of ultra-sectionning in images:''' 400px|left|thumb|1. Trimming resin block using Trim diamond knife<br /> [[File:8 (2).jpg|400px|left|thumb|2. Ul..." |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Procedure of ultra-sectionning | '''Procedure of ultra-sectionning''' | ||
[[File:1.jpg|400px|left|thumb|1. Trimming resin block using Trim diamond knife]]<br /> | [[File:1.jpg|400px|left|thumb|1. Trimming resin block using Trim diamond knife]]<br /> | ||