Fig 2: Sketch of subsequent platinum deposition. | Fig 2: Sketch of subsequent platinum deposition. | ||
[[File:fig3_1.tif]][[File:fig3_2.tif]] | [[File:fig3_1.tif|800px]][[File:fig3_2.tif|800px]] | ||
Fig 3: SE images acquired before and after electron beam deposited platinum. | Fig 3: SE images acquired before and after electron beam deposited platinum. | ||
When a suitable region of interest has been located selected by SEM, it is necessary to protect | When a suitable region of interest has been located selected by SEM, it is necessary to protect | ||
the surface from damage from the ion beam. A typical deposition scheme is illustrated on | the surface from damage from the ion beam. A typical deposition scheme is illustrated on | ||