Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of NiFe: Difference between revisions

Reet (talk | contribs)
Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thi..."
 
Reet (talk | contribs)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_NiFe click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_NiFe click here]'''


==Sputtering of Nickel Iron alloy==
==Deposition of Nickel Iron alloy==


Nickel Iron has been sputter deposited in the [[Specific_Process_Knowledge/Thin_film_deposition/Lesker|Sputter-system (Lesker)]] here at Nanolab.
Nickel Iron has previously been sputter deposited in the [[Specific_Process_Knowledge/Thin_film_deposition/Lesker|Sputter-system (Lesker)]] here at Nanolab.


Read more about process parameters and previous results of sputtering Ni-Fe in the Lesker sputter system [[/Sputtering of NiFe in the Lesker sputter system|here]].
Read more about process parameters and previous results of sputtering Ni-Fe in the Lesker sputter system [[/Sputtering of NiFe in the Lesker sputter system|here]].