Specific Process Knowledge/Thin film deposition/Deposition of Platinum: Difference between revisions
New page: Platinum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. {| border="1" cellspacing="0" cellpadding="4" ! ! E-beam evapora... |
No edit summary |
||
Line 4: | Line 4: | ||
{| border="1" cellspacing="0" cellpadding="4" | {| border="1" cellspacing="0" cellpadding="4" | ||
! | ! | ||
! E-beam evaporation (Alcatel) | ! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Alcatel|Alcatel]]) | ||
! E-beam evaporation (Leybold) | ! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Leybold|Leybold]]) | ||
! E-beam evaporation (Wordentec) | ! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]]) | ||
|- | |- | ||
| Batch size | | Batch size |
Revision as of 14:43, 5 February 2009
Platinum can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.
E-beam evaporation (Alcatel) | E-beam evaporation (Leybold) | E-beam evaporation (Wordentec) | |
---|---|---|---|
Batch size |
|
|
|
Pre-clean | RF Ar clean | Ar ion bombartment | RF Ar clean |
Layer thickness | 10Å to 1µm | 10Å to 1500 Å | 10Å to 1 µm |
Deposition rate | 2Å/s to 15Å/s | 1Å/s to 5Å/s | 10Å/s to 15Å/s |