{| border="1" cellspacing="0" cellpadding="4"  
{| border="1" cellspacing="0" cellpadding="4"  
!  
!  
! E-beam evaporation (Alcatel)
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Alcatel|Alcatel]])
! E-beam evaporation (Leybold)
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Leybold|Leybold]])
! E-beam evaporation (Wordentec)
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]])
! Sputter deposition (Wordentec)
! Sputter deposition ([[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]])
|-  
|-  
| Batch size
| Batch size