| Line 58: | Line 58: | ||
# How do we know if something that is very brief happens? For instance, spikes in reflected power can be rather short lived as indicated by the one point spikes of reflected coil power above. | # How do we know if something that is very brief happens? For instance, spikes in reflected power can be rather short lived as indicated by the one point spikes of reflected coil power above. | ||
In both cases, the sampling frequency of 2 Hz is simply not high enough - we need to increase this. The SPTS Pro software can only lower this. However, realizing that all the devices (mass flow controllers, pressure gauges, RF generators etc.) responsible for the parameters in the plot above are produce output measurements in real time, we can sample these parameters by some external device. Enter the | In both cases, the sampling frequency of 2 Hz is simply not high enough - we need to increase this. The SPTS Pro software can only lower this. However, realizing that all the devices (mass flow controllers, pressure gauges, RF generators etc.) responsible for the parameters in the plot above are produce output measurements in real time, we can sample these parameters by some external device. Enter the | ||
[https://www.picotech.com/oscilloscope/4824/8-channel-oscilloscope Picoscope oscilloscope] with 8 analog channels that enable us sample up to 8 outputs, usually a DC voltage, at almost any sampling rate. Unlike the old oscilloscopes, the Picoscope is fully operated by a software that produces a vast amount of data and nice plots. We therefore have to decide which parameters are most important to monitor and then go through the electrical diagrams to find an appropriate place to pick up the signal. | [https://www.picotech.com/oscilloscope/4824/8-channel-oscilloscope Picoscope oscilloscope] with 8 analog channels that enable us sample up to 8 outputs, usually a DC voltage, at almost any sampling rate. Unlike the old oscilloscopes, the Picoscope is fully operated by a software that produces a vast amount of data and nice plots. We therefore have to decide which process parameters are the most important to monitor and then go through the electrical diagrams to find an appropriate place to pick up the signal. This set of parameters is chosen as shown in the plots above. | ||
This set of parameters chosen | |||
Comparing the two plots we observe the following: | |||
* There is, indeed, short lived incidences that are not picked up by the SPTS Pro software: | |||
** Spikes of high flow when the C<sub>4</sub>F<sub>8</sub> MFC opens. | |||
** Spikes of reflected coil power. | |||
** The reading of the DC Bias has much more detail than the one-point reading of the Pro software indicates. | |||
* There are oscillations in the pressure every time whenever there is a change of gas flow | |||