Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/picoscope: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
Jmli (talk | contribs)
Line 37: Line 37:


<gallery caption="4 cycles of Process A " widths="400" heights="500" perrow="2">
<gallery caption="4 cycles of Process A " widths="400" heights="500" perrow="2">
image:Process A SPTS.png | Recorded with the SPTS software
image:Process A SPTS.png | Left: Recorded with the SPTS software
image:Process A pico.png | Recorded with the Picoscope
image:Process A pico.png | Right: Recorded with the Picoscope
</gallery>
</gallery>


<gallery caption="4 cycles of Process D4 " widths="400" heights="500" perrow="2">
<gallery caption="4 cycles of Process D4 " widths="400" heights="500" perrow="2">
Image:PrD4 SPTS.png | Recorded with the SPTS software
Image:PrD4 SPTS.png | Left: Recorded with the SPTS software
Image:PrD4 pico.png |Recorded with the Picoscope
Image:PrD4 pico.png | Right: Recorded with the Picoscope
</gallery>
</gallery>



Revision as of 12:16, 17 March 2020

Process optimization using the Picoscope

The original standard recipes on Pegasus 1 differ in many ways. The second step of one of them is listed below:

Process A Step 2 parameters
Parameter Etch Dep
Gas flow (sccm) SF6 350 (1.5 s), 550 C4F8 200
Cycle time (secs) 7.0 4.0
Pressure (mtorr) 25 (1.5 s), 150 25
Coil power (W) 2800 2000
Platen power (W) 140 (1.5) 45 0
Common Temperature 20 degs


4 cycles of the recipe PrD4 recorded with the Picoscope
4 cycles of the recipe PrD4 recorded with the SPTS software
4 cycles of the recipe Prcocess A recorded with the Picoscope
4 cycles of the recipe PrD4 recorded with the SPTS software