Line 3: Line 3:
The Pegasus tools were delivered with a set of standard recipes
The Pegasus tools were delivered with a set of standard recipes


<gallery caption="4 cycles of Process A " widths="532" heights="620" perrow="2">
<gallery caption="4 cycles of Process A " widths="400" heights="500" perrow="2">
image:Process A SPTS.png | Recorded with the SPTS software
image:Process A SPTS.png | Recorded with the SPTS software
image:Process A pico.png | Recorded with the Picoscope
image:Process A pico.png | Recorded with the Picoscope

Revision as of 12:41, 17 March 2020

Process optimization using the Picoscope

The Pegasus tools were delivered with a set of standard recipes


4 cycles of the recipe PrD4 recorded with the Picoscope
4 cycles of the recipe PrD4 recorded with the SPTS software
4 cycles of the recipe Prcocess A recorded with the Picoscope
4 cycles of the recipe PrD4 recorded with the SPTS software