Revision as of 12:22, 17 March 2020
Feedback to this page: click here
Molybdenum deposition
Molybdenum can be deposited by e-beam evaporation or sputtering. In the chart below you can compare the different deposition equipment.
| E-beam evaporation (Temescal) | Sputter deposition (Lesker) | |
|---|---|---|
| General description | E-beam deposition of Mo
(line-of-sight deposition) |
Sputter deposition of Mo
(not line-of-sight) |
| Pre-clean | Ar ion source | RF Ar clean |
| Layer thickness | 10Å to 0.6 µm* | 10Å to 500 Å |
| Deposition rate | 1Å/s to 10Å/s | Depends on process parameters, roughly about 1 Å/s |
| Batch size |
|
|
| Allowed materials |
|
|
| Comment | As of August 2018, Mo has not yet been deposited in the Temescal.
Please contact the Thin Film group to develop a process. |
* If depositing more than 600 nm in total, write to metal@danchip.dtu.dk well in advance to ensure enough material is present.